Home / Products / Nickel Alloys / Inconel 625 / ASTM B366 Inconel 625 Threaded Fittings
Inconel 625 (UNS: N06625, Werkstoff Nr.: 2.4856)
Fabricated using stainless steel, our range of threaded fittings is one of the most demanded items of our entire range. Suitable for different industrial projects, these adroitly developed threaded pipe fittings are stringently checked for their durability and strength. These are also offered in accordance with the national and international standard & specifications.
ASTM B366 Inconel 625 Threaded Fittings
Specifications
Standards | Designation |
ASTM | B 366 |
ASME | SB 366 |
UNS | N06625 |
Werkstoff Nr. | 2.4856 |
Dimensions
- 90° Elbow
- 45° Elbow
- Tee
- Cross
- Full Coupling
- Half Coupling
- Reducing Coupling
- Pipe Cap
- Hex Head Bushing
- Hex Head Plug
- Square Head Plug
- Round Head Plug
- Union
- Hex Nipple
- Street Elbow
- Bull Plug
- Boss
- Swage Nipple
- Pipe Nipple
- Adapter
- Union (Male x Female)
- Branch Outlet
- 90° Elbow Outlet
- 45° Lateral Tee
- Lateral Outlet
- Nipple Branch Outlet
- SCREWED FITTINGS - B16.11 / BS3799 Weight
Chemical Composition
Inconel 625 | |
Ni | 58.0 min |
Cr | 20.0 – 23.0 |
Fe | 5.0 max |
C | 0.10 max |
Mn | 0.50 max |
Si | 0.50 max |
Mo | 8.0 – 10.0 |
Co | 1.0 max |
Al | 0.40 max |
Ti | 0.40 max |
Nb + Ta | 3.15 – 4.15 |
P | 0.015 max |
S | 0.015 max |
Mechanical & Physical Properties – Inconel 625
Density | 8.4 g/cm3 |
Melting Point | 1350 °C (2460 °F) |
Tensile Strength | Psi – 135,000 , MPa – 930 |
Yield Strength (0.2%Offset) | Psi – 75,000 , MPa – 517 |
Elongation | 42.5 % |
Subcategory: Metal; Nickel Base; Superalloy
Key Words: ASME SB-443, SB-444, SB-446, SB-564, Boiler Code Sections I, III, VIII, IX; AFNOR NC 22 D Nb; VdTUV 499, AMS 5581, AMS 5599, AMS 5666, AMS 5837; DIN 17744, 17750-17752, 17754; Werkstoff Nr. 2.4856; NACE MR-01-75, UNS N06625; BS 3072, 3074, 3076 (NA21); ASTM B443, ASTM B444, ASTM B446, ASTM B564, ASTM B704, ASTM B705, ASTM B751
Component Al C Co Cr Fe |
Wt. % Max 0.4 Max 0.1 Max 1 20 - 23 Max 5 |
Component Mn Mo Nb Ni |
Wt. % Max 0.5 8 - 10 3.15 - 4.15 Min 58 |
Electrical Properties | |||
Electrical Resistivity | 0.000129 ohm-cm | 0.000129 ohm-cm | |
Magnetic Permeability | 1.0006 | 1.0006 | at 200 oersted (15.9 kA/m) |
Curie Temperature | Max -196 °C | Max -321 °F | |
Thermal Properties | |||
CTE, linear 20°C | 12.8 µm/m-°C | 7.11 µin/in-°F | 20-100°C |
Heat Capacity | 0.41 J/g-°C | 0.098 BTU/lb-°F | |
Thermal Conductivity | 9.8 W/m-K | 68 BTU-in/hr-ft²-°F | |
Melting Point | 1290 - 1350 °C | 2350 - 2460 °F | |
Solidus | 1290 °C | 2350 °F | |
Liquidus | 1350 °C | 2460 °F |
Main Export Market
- Eastern Europe
- North America
- Mid East/Africa
- Central/South America
- Asia
- Western Europe
- Australasia
- UAE
U.A.E,
Oman,
Saudi Arabia,
Qatar,
Bahrain,
Egypt,
Turkey
Singapore,
Thailand,
Malaysia
Indonesia
Poland
Italy
Portugal
Spain
Brazil
Chile
Venezuela
Costa Rica
USA
Canada
Angola
Sri Lanka
Russia